This PhD thesis develops new chemical precursors for Atomic Layer Deposition (ALD), focusing on cobalt and nickel silylamido complexes. In collaboration with BASF, their properties in solution, solid, and gas phases are studied to evaluate their suitability for ALD. Additionally, deposition experiments of tantalum and molybdenum chalcogenides explore ALD’s potential in electrochemical water splitting applications.

39,90 €

In past decades, miniaturization of materials was immanent in all fields of technology, especially in semiconductor industry. Nowadays, miniaturization of semiconducting compounds reached a level where established manufacturing processes reach their technical limits. Atomic Layer Deposition (ALD) offers an alternative method for the deposition of ultra-thin metallic films, which is a crucial step in the fabrication of semiconducting compounds. Based on a chemical reaction between surface and gas phase, ALD is a process which touches both synthetic chemistry and material sciences.
This PhD thesis focuses on the development of new chemicals for the use as precursor in ALD. Within a research and development cooperation with BASF, the properties of a new series of cobalt and nickel silylamido complexes in solution, in the solid state and in the gas phase are studied and evaluated with respect to their use as ALD precursor. Furthermore, deposition experiments of tantalum and molybdenum chalcogenides were performed to test the application of ALD in the field of electrochemical water splitting.

Auflage

1

EAN

9783863761820

ISBN

978-3-86376-182-0

Titel

Design of Metal-Organic Molecular Precursors for Atomic Layer Deposition

Kurztitel

Atomic Layer Deposition

Autor

Organisation

Georg-August Universität Göttingen

Gutachter

,

Erscheinungsdatum

21.12.2020

Erscheinungsjahr

2020

Verlag

Ort

Göttingen

Ausgabeart

Softcover

Sprache

englisch

Seiten

143

Medium Buch
Produkttyp

Dissertation

ISNI Dr. Jan Gerkens (Autor): 0000-0005-1617-079X

Herstellerinformationen

Sievers & Partner
Erfurter Str. 10
96450 Coburg
Deutschland (Bayern)
Tel: +49 9561 6754754
E-Mail: info@elitebuch.com

Alle auf dieser Seite angebotenen Produkte entsprechen den geltenden gesetzlichen Vorschriften zur Produktsicherheit gemäß der Verordnung (EU) 2023/988 über die allgemeine Produktsicherheit (GPSR).

Exportformate